KYPICR/KYPIFCR |
¡¡
¡¡
|
¡¡
|
Properties
¡¡ Polyimide FCR Film(KYPIFCR) is Polyimide corona-resistant film coated with FEP resin on one side(FH) through the sintering process at high temperature, which combines the excellent properties of Polyimide corona-resistant film and FEP resin. It can be widely applied for winding insulation of magnet wires for H~C class traction motors , high-voltage motors and generators etc. |
Main Specification
|
Items |
unit |
KYPICR |
KYPIFCR |
|
|
Thickness |
mm(mil) |
0.025(1) |
0.038(1.5) |
|
|
Tolerance of thickness |
mm |
¡À0.002 |
¡À0.003 |
|
|
Witdh |
mm |
6¡«520 |
6¡«500 |
|
|
Tolerance of width |
mm |
¡À0.4¡«¡À2.0 |
¡À0.4¡«¡À2.0 |
|
|
*Corona resistance, hr at voltage1KV, frequency 20KHz temperature 90¡æ¡À2¡æ, pulse rise time 400ns |
h |
¡Ý50 |
¡Ý50 |
|
|
Tensile Stength |
MPa (psi¡Á103) |
¡Ý120(17.4) |
¡Ý80(11.6) |
|
|
Elongation at rupture |
% |
¡Ý40 |
¡Ý40 |
|
|
Shrinkage |
150¡æ,0.5h |
% |
¡Ü1.0 |
¡Ü1.0 |
|
400¡æ,0.5h |
¡Ü3.0 |
¡Ü3.0 |
||
|
Peel Strength (F¨CF) |
N/25mm(g/cm) |
-- |
¡Ý6.0(245) |
|
|
Breakdown Strength |
MV/M(V/mil) |
¡Ý 200(5080) |
¡Ý 120(3048) |
|
|
*Surface Resistivity 200+/5c(392F) |
¦¸¡¤cm |
¡Ý1¡Á1015 |
¡Ý1¡Á1015 |
|
|
*Volume Resistivity 200+/-5c(392F) |
¦¸ |
¡Ý1¡Á1015 |
¡Ý1¡Á1015 |
|
|
* Dielectric constant(48¡«62Hz) |
-- |
3.5¡À0.4 |
3.5¡À0.4 |
|
|
* Loss tangent(48¡«62Hz) |
-- |
¡Ü3.5¡Á10-3 |
¡Ü3.5¡Á10-3 |
|
| ¡¡ Note: The items marked * are the inherent properties of Polyimide Film, which are not showed on the testing report for outgoing factory.
|
¡¡
|